Problem 86
Question
Superalloys have been made of nickel and aluminum. The alloy owes its strength to the formation of an ordered phase, called the gamma-prime phase, in which Al atoms are at the corners of a cubic unit cell and Ni atoms are at the face centers. What is the composition (relative numbers of atoms) for this phase of the nickel–aluminum superalloy?
Step-by-Step Solution
Verified Answer
The composition of the gamma-prime phase of the nickel-aluminum superalloy in terms of the relative numbers of atoms is 1 Al atom and 3 Ni atoms, which can be represented as Al : Ni = 1:3.
1Step 1: 1. Collect the information
We know that aluminum atoms are at the corners of the unit cell (8 corners) and nickel atoms are at the face centers (6 faces) of the cubic unit cell.
2Step 2: 2. Calculate the number of Al atoms in the unit cell
Each corner atom of the cubic unit cell is shared by 8 different cells. Since there are 8 corner positions in the unit cell, the total number of Al atoms contributed to the unit cell is (8 corners x (1/8)) = 1 Al atom.
3Step 3: 3. Calculate the number of Ni atoms in the unit cell
Each face-centered atom of the cubic unit cell is shared by 2 different cells. Since there are 6 face center positions in the unit cell, the total number of Ni atoms contributed to the unit cell is (6 faces x (1/2)) = 3 Ni atoms.
4Step 4: 4. Determine the composition
The composition of the gamma-prime phase of the nickel-aluminum superalloy in terms of the relative numbers of atoms can be given as: 1 Al atom and 3 Ni atoms. This can be simplified by removing the units and stating the composition as Al : Ni, which is 1:3.
Key Concepts
Gamma-Prime PhaseCubic Unit CellNickel-Aluminum AlloyAtomic Composition
Gamma-Prime Phase
The gamma-prime phase is a significant aspect of nickel-based superalloys, crucial to their strength and stability at high temperatures. In these superalloys, the gamma-prime phase is an ordered phase where aluminum and nickel atoms form a specific arrangement.
This arrangement is known for its distinctive crystal structure, which enhances the alloy's overall properties.
In this phase, aluminum atoms are positioned at the corners of a crystal structure known as a cubic unit cell. Nickel atoms, on the other hand, occupy the face-centered positions.
This structure helps in blocking dislocation movements, making the alloy super strong and resistant to deformation.
The importance of the gamma-prime phase lies in its ability to provide increased creep resistance and strength to the superalloy, especially when exposed to harsh operating conditions such as those in jet engines and gas turbines.
By understanding and manipulating the gamma-prime phase, researchers can engineer materials with desired properties for advanced applications.
This arrangement is known for its distinctive crystal structure, which enhances the alloy's overall properties.
In this phase, aluminum atoms are positioned at the corners of a crystal structure known as a cubic unit cell. Nickel atoms, on the other hand, occupy the face-centered positions.
This structure helps in blocking dislocation movements, making the alloy super strong and resistant to deformation.
The importance of the gamma-prime phase lies in its ability to provide increased creep resistance and strength to the superalloy, especially when exposed to harsh operating conditions such as those in jet engines and gas turbines.
By understanding and manipulating the gamma-prime phase, researchers can engineer materials with desired properties for advanced applications.
Cubic Unit Cell
A cubic unit cell is the simplest repeating unit of a crystal structure, forming the building block of the material's lattice. In simple cubic, body-centered cubic, and face-centered cubic structures, cubic unit cells play a fundamental role in dictating the properties of materials.
For the gamma-prime phase of nickel-aluminum superalloys, the unit cell is specifically a face-centered cubic (FCC) structure.
In this structure:
The cubic unit cell is crucial because its geometric arrangement influences the packing efficiency and the resulting material properties.
For the gamma-prime phase of nickel-aluminum superalloys, the unit cell is specifically a face-centered cubic (FCC) structure.
In this structure:
- Aluminum atoms are located at the corners of the unit cell, and each of these corner atoms is shared among eight neighboring cells.
- Nickel atoms are situated at the center of each face of the cube, and these face-centered atoms are shared between two unit cells.
The cubic unit cell is crucial because its geometric arrangement influences the packing efficiency and the resulting material properties.
Nickel-Aluminum Alloy
Nickel-aluminum alloys are widely recognized for their mechanical strength and resistance to high temperatures and oxidation. These alloys are frequently employed in demanding environments such as aerospace and power generation industries.
In these types of alloys, aluminum is often added to nickel to enhance properties such as strength and durability. The formation of the gamma-prime phase is particularly valuable in these alloys because it significantly reinforces the alloy, providing outstanding temperature and creep resistance.
The nickel content within the alloy contributes to its high melting point and excellent resistance to corrosion and oxidation. Meanwhile, aluminum helps in forming the ordered gamma-prime phase, which is crucial in strengthening the alloy.
The nickel-aluminum alloy stands out as one of the most effective materials for high-performance applications thanks to this unique combination and structural arrangement, offering a balance between toughness and durability.
In these types of alloys, aluminum is often added to nickel to enhance properties such as strength and durability. The formation of the gamma-prime phase is particularly valuable in these alloys because it significantly reinforces the alloy, providing outstanding temperature and creep resistance.
The nickel content within the alloy contributes to its high melting point and excellent resistance to corrosion and oxidation. Meanwhile, aluminum helps in forming the ordered gamma-prime phase, which is crucial in strengthening the alloy.
The nickel-aluminum alloy stands out as one of the most effective materials for high-performance applications thanks to this unique combination and structural arrangement, offering a balance between toughness and durability.
Atomic Composition
Understanding the atomic composition of materials is key to controlling their properties and eventual use. The atomic composition refers to the relative number of each type of atom present in a compound or alloy.
In the gamma-prime phase of nickel-aluminum superalloys, the atomic composition is described by the proportion of aluminum to nickel atoms within the unit cell.
The nickel-aluminum alloy features aluminum atoms located at the corners of a cubic unit cell and nickel atoms at the face centers.
From calculations based on their positions in the cubic unit cell:
By manipulating the atomic composition, engineers and scientists can create materials tailored for specific applications and desired characteristics.
In the gamma-prime phase of nickel-aluminum superalloys, the atomic composition is described by the proportion of aluminum to nickel atoms within the unit cell.
The nickel-aluminum alloy features aluminum atoms located at the corners of a cubic unit cell and nickel atoms at the face centers.
From calculations based on their positions in the cubic unit cell:
- 1 aluminum atom is contributed by the corners due to the sharing of the corner atoms.
- 3 nickel atoms are contributed by the face centers, each face-centered nickel atom being shared between two cells.
By manipulating the atomic composition, engineers and scientists can create materials tailored for specific applications and desired characteristics.
Other exercises in this chapter
Problem 84
What type of solid will each of the following substances form? a. diamond b. \(\mathrm{PH}_{3}\) c. \(\mathrm{H}_{2}\) d. \(\mathrm{Mg}\) e. \(\mathrm{KCl}\) f.
View solution Problem 85
The memory metal, nitinol, is an alloy of nickel and titanium. It is called a memory metal because after being deformed, a piece of nitinol wire will return to
View solution Problem 95
Diethyl ether \(\left(\mathrm{CH}_{3} \mathrm{CH}_{2} \mathrm{OCH}_{2} \mathrm{CH}_{3}\right)\) was one of the first chemicals used as an anesthetic. At \(34.6^
View solution Problem 96
Mercury is the only metal that is a liquid at room temperature. When mercury vapor is inhaled, it is readily absorbed by the lungs, causing significant health r
View solution